Why I abuse batteries was: trojan battery cycle [RE-wrenches]

Bob Ellison reellison at gmail.com
Sat Feb 16 06:01:15 PST 2008


It is really simple, the bubbles get lifted into the hydrometer and
make the fload read higher than it would otherwise.

 bob


On Feb 15, 2008 11:46 AM, Allan Sindelar <allan at positiveenergysolar.com> wrote:
>
> Drake,
> I have long understood that the bubbles created by the gassing action during
> charging stirs up and destratifies the electrolyte. Is that what you're
> referring to?
> Allan at PosE
>
>
> ----- Original Message -----
> From: "Drake Chamberlin" <Drake.Chamberlin at redwoodalliance.org>
> >
> > It seems that the specific gravity is affected by bubbles in the
> > electrolyte during charge.  I've heard this from others, and it
> > appears to be true from my observation.   Does anyone have any data
> > on this effect?
> >
>
>
>
> - - - -
> Hosted by Home Power magazine
>
> To send a message: RE-wrenches at topica.com
>
> Archive of previous messages: http://lists.topica.com/lists/RE-wrenches/read
>
> List rules & how to change your email address: www.mrsharkey.com/wrenches/etiquette.php
>
> Check out participant bios: www.mrsharkey.com/wrenches/
>
> Moderator: michael.welch at homepower.com
>
>
>



More information about the RE-wrenches mailing list