[RE-wrenches] Strings and series of batteries
Windsun@wind-sun.com
windsun at wind-sun.com
Wed Dec 2 17:07:24 PST 2009
Yes, I hate Vaseline - it has a melting point of around 105 deg F, so even a
moderatly hot day will cause it to drip all over the place - except onto the
terminals it is supposed to protect.
..................................................................................................
Northern Arizona Wind & Sun - Electricity From The Sun Since 1979
Solar Discussion Forum: http://www.wind-sun.com/ForumVB/
..................................................................................................
----- Original Message -----
From: "Larry Crutcher, Starlight Solar" <larry at starlightsolar.com>
To: "RE-wrenches" <re-wrenches at lists.re-wrenches.org>
Sent: Wednesday, December 02, 2009 5:27 PM
Subject: Re: [RE-wrenches] Strings and series of batteries
> Another YES for silicon. We have used it for years. A very thin coat will
> last a long time. I have seen the gooey mess for heated vaseline more
> than once.
>
> Larry
>